Shear flocculation of celestite with sodium oleate and tallow amine acetate: effects of cations

J Colloid Interface Sci. 2004 May 1;273(1):170-4. doi: 10.1016/j.jcis.2004.01.045.

Abstract

Sodium oleate and tallow amine acetate (TAA) were used as surfactants for the shear flocculation of celestite. The shear-flocculation power values obtained with sodium oleate were higher than those obtained with TAA in terms of the concentrations used in the shear-flocculation experiments. In addition, sodium oleate and TAA were more effective on the celestite suspension in the pH ranges of 7-11 and 6-10, respectively. For the shear-flocculation experiments with sodium oleate at pH 11, with preaddition of calcium or magnesium ions at 5 x 10(-5) M and lower concentrations into the suspension, the shear flocculation of the celestite suspension was promoted by the coagulation process due to the calcium and magnesium cations added. However, the shear-flocculation power values decreased due to the interaction between surfactant and cations at concentration values higher than 5 x 10(-5) M for magnesium ions and 10(-3) M for calcium ion. Particularly, magnesium ions significantly reduced the shear-flocculation power values by slime coating of Mg(OH)2 precipitates.