Evaluation of the Surface Irregularities of the Cross-Section of the Wood after CO2 Laser Cutting

Materials (Basel). 2023 Nov 15;16(22):7175. doi: 10.3390/ma16227175.

Abstract

The present paper deals with the analysis of cross-section surface irregularities after CO2 laser cutting. The surface irregularities of beech (Fagus sylvatica L.), oak (Quercus petraea), and spruce (Picea abies L.) wood were quantified by primary profile parameters using a digital microscope. The arithmetic mean height (Pa), used as the basic parameter, was supplemented by amplitude parameters (Pv, Pp, Pz) and the Psm parameter, through which the shape of the irregularity was specified in more detail. A statistically significant change was demonstrated when changing the values of the feed speed and the power of the CO2 laser. The results of this article confirm that the surface irregularities increased with an increasing laser power and decreasing feed rate. The scanned topographic images also provide a more detailed explanation of the measured P-parameters and point out the risks associated with the evaluation of the cross-section with the primary profile.

Keywords: CO2 laser cutting; cross-section; digital microscope; primary profile; surface irregularities.