Relationship between air-blowing duration and bond strengths of three adhesive systems to dentin after thermal aging.
Daneshmehr L, Ozer F, Mante FK, Blatz MB.
Daneshmehr L, et al.
Dent Mater J. 2013;32(5):767-74. doi: 10.4012/dmj.2013-026.
Dent Mater J. 2013.
PMID: 24088832
Free article.
Bonded surfaces from each group were air-blown for 0, 5, or 10 s and cured. Composite cylinders were built on the treated surfaces and cured. Half of the specimens from each group were tested immediately and the other halves were tested after thermal aging. Statistical ana …
Bonded surfaces from each group were air-blown for 0, 5, or 10 s and cured. Composite cylinders were built on the treated surfaces an …