High concentration of residual aluminum oxide on titanium surface inhibits extracellular matrix mineralization
Canabarro A, et al. J Biomed Mater Res A 2008. Among authors: Rosa AL. PMID 18186053
Five different surfaces were evaluated: ground (G), ground and chemical etched (G1-HF for 60 s), sand blasted (SB-Al(2)O(3) particles 65 mum), sand blasted and chemical etched (SLA1-HF for 60 s and SLA2-HF for 13 s). ...Al(2)O(3) residues were detected on SB and SLA2 surfaces. Only matrix mineralization formation was affected by different surface treatments, being increased on rough surface (SLA1) and reduced on surface with high amount of Al(2)O(3) residues (SB). ...
Five different surfaces were evaluated: ground (G), ground and chemical etched (G1-HF for 60 s), sand blasted (SB-Al(2)O(3) particles …